Polymer Property : Tensile Strength, Yield = 7690 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East)
High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Strength, Yield 53.0 MPa
7690 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS
Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press.
Tensile Strength, Yield 53.0 MPa
7690 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Tensile Strength, Yield 53.0 MPa
7690 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ML7647 PC
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 53.0 MPa
7690 psi
ISO 527
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Cycolac® BDT5510 ABS
Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only.
Tensile Strength, Yield 53.0 MPa

@Thickness 6.35 mm
7690 psi

@Thickness 0.250 in
ASTM D638
SABIC Innovative Plastics Lexan® FL2000 PC
Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled PC.
Tensile Strength, Yield 53.0 MPa
7690 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal
LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66
LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact.
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 53.0 MPa
7690 psi
50 mm/min; ISO 527
SABIC Innovative Plastics NORYL PVX0800 PPE
NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications.
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL EM6101 PPE+PS
Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range.
Tensile Strength, Yield 53.0 MPa
7690 psi
ISO 527
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Tensile Strength, Yield 53.0 MPa
7690 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339G20M10CL Glass/Mineral Reinforced Coupled
Tensile Strength, Yield 53.0 MPa

@Temperature 80.0 °C
7690 psi

@Temperature 176 °F
ISO Data
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade.
Tensile Strength, Yield 53.0 - 57.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
7690 - 8270 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 53.0 MPa
7690 psi
ISO 527
Azoty Tarnow™ TARNOFORM 300 DW POM
Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor..
Tensile Strength, Yield 53.0 MPa
7690 psi
Ineos ABS NOVODUR® P3T ABS, Injection Grade  (discontinued **)
Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Tensile Strength, Yield 53.0 MPa
7690 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..