| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527-1 |
|
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50% RH; ISO 527-1 |
|
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific)
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46
LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA
LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP DFB03GR PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DFB03GR is a compound based on Polycarbonate resin containing a mixture of Glass Fiber and Glass Beads. Added features of this material include: Easy Molding.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific)
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL PX4716 PPE+HIPS (Asia Pacific)
PPE+PS GF15% FR V-1
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | DIN EN ISO 527 |
|
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | Elastic Limit |
|
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | GB/1040 |
|
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66
Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded
Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
|
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded
Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | |
|
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO R527 |
|
Arkema Group Orgalloy® RS 6015 ES T6L Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527 |
|
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural
High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | |
|
Asahi Kasei Xyron® G701V Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527 |
|
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min |
|
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade
(discontinued **)
OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface ..
|
|||