| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | Type I, 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527 |
|
Eastman 9921P PET Injection Molded
(discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
|
|||
| Tensile Strength, Yield |
54.0
MPa @Thickness 6.35 mm |
7830
psi @Thickness 0.250 in |
ASTM D638 |
|
SABIC Innovative Plastics Lexan® FL403 PC
Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"".
|
|||
| Tensile Strength, Yield |
54.0
MPa @Thickness 6.35 mm |
7830
psi @Thickness 0.250 in |
ASTM D638 |
|
SABIC Innovative Plastics Lexan® FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
Global PC/ABS-1218 Standard PC/ABS Grade
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRILOY D2000P PC
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS
NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East)
XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527-2 |
|
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin
Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific)
PPE+PS, HDT 125
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527 |
|
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 21% Glass Spray-up Laminate |
|
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527 |
|
Chi Mei Polylac® PA-757 ABS
High gloss, medium impact
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® 300TE BK602 Acetal (POM)
(Unverified Data**)
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE BK602 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 23°C, 50% RH; ASTM D638 |
|
Asahi Kasei Xyron® 500V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527 |
|
BASF Ultramid® A3K Q603 PA66 (Conditioned)
Description: Ultramid A3K Q603 is a general purpose PA6/6.Information provided by BASF
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
|
Ashley Polymers Ashlene® RH190ST Acetal
A high impact homopolymer resin.Data provided by the manufacturer
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
|
|||
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
|
|||