Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 8100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade
Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant
Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Tensile Strength, Yield 55.8 - 172 MPa
8100 - 24900 psi
Average value: 79.1 MPa Grade Count:46
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES Elastoblend® PA6/66 IM 6040 MB
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES Electrablend® PC/ABS
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc.
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES Electrablend® PC/ABS 033009
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc.
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES HiFill FR® PA6/6 FR 344
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES Luriblend® PA6 TL25 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (25%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 55.8 MPa
8100 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate
EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Styron CALIBREâ„¢ IM 401-11 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D-638
Axiall ProTherm® 4510 CPVC Rigid PVC, Molding
Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high che..
Tensile Strength, Yield 55.8 - 145 MPa
8100 - 21000 psi
Average value: 83.2 MPa Grade Count:10
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Techmer ES HiFill FR® PA6/6 FR 344 BK
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved