| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 0.680 GPa | 98.6 ksi | ISO 527-2/1A |
|
Polymer Industries Polyslick UHMW Rod
Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | ISO 527-2/1A |
|
Polymer Industries Polyslick UHMW Sheet
Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material ..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | ISO 527-2/1A |
|
Polymer Industries Polyslick UHMW Profile
Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p..
|
|||
| Tensile Modulus |
0.680
GPa @Temperature 40.0 °C |
98.6
ksi @Temperature 104 °F |
DAM; ISO 11403-1 -2 |
|
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | ISO R 527 |
|
Arkema Group OREVAC® 18750 Maleic Anhydride Modified Polypropylene
DescriptionOREVAC 18750 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | ASTM D638 |
|
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | |
|
Addcomp PRIEX® 25050 Maleic Anhydride Grafted PP random copolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | |
|
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | 1 mm/min |
|
Arkema Group Kynar® FLEX 2821 PVDF
(discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn..
|
|||
| Tensile Modulus | 0.680 GPa | 98.6 ksi | 1 mm/min |
|
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness ..
|
|||