Polymer Property : Tensile Modulus = 1.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 GPa
145 ksi
STN EN ISO 527-2
Plastcom PLASTAMID® 6 HI PA6 with improved impact strength
PA 6 for injection molding, impacted, modified with thermoplastic elastomer, determined for high impacted moldings also at low temperature. Delivered in natural mode and in the full RAL color scale...
Tensile Modulus 1.00 GPa
145 ksi
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,..
Tensile Modulus 1.00 GPa
145 ksi
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade
Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm..
Tensile Modulus 1.00 GPa
145 ksi
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade
Easy-to-process blow molding grade for stackable canisters (up to 60 l), used for packing surface-active liquids, laundry and dishwashing detergents, disinfectants, drums (up to 220 l) for various s..
Tensile Modulus >= 1.00 GPa
>= 145 ksi
ASTM D638
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE
Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®.
Tensile Modulus >= 1.00 GPa
>= 145 ksi
ASTM D638
Forever Plast Namtene® Recycled Standard HDPE
Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1
Iran Petrochemical (PCC) HB5020 High Density Polyethylene
HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co.
Tensile Modulus 1.00 GPa
145 ksi
DIN 53457
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene
Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH
Tensile Modulus 1.00 - 1.50 GPa
145 - 218 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope..
Tensile Modulus 1.00 GPa
145 ksi
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..
Tensile Modulus 1.00 GPa
145 ksi
1mm/min; ISO 527-2
Borealis BL1481 High Density Polyethylene
BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular..
Tensile Modulus 1.00 GPa
145 ksi
At 1 mm/min; ISO 527-2
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding
Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig..
Tensile Modulus 1.00 GPa
145 ksi
MD; ASTM D882-A
Borealis FS1560 High Density Polyethylene
FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala..
Tensile Modulus 1.00 GPa
145 ksi
ISO 527
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene
This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity an..
Tensile Modulus 1.00 GPa
145 ksi
ISO 572-2
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a..
Tensile Modulus 1.00 GPa
145 ksi
MD; ASTM D882-A
Borealis FS1470 High Density Polyethylene
FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala..
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
DSM Stanyl® TE373 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 1.00 GPa
145 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 1.00 GPa
145 ksi
cond; ISO 527-1/-2
DSM Stanyl® TS300 PA46
Tensile Modulus 1.00 GPa
145 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America)
Information provided by DSM Engineering Plastics.
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America)
Information provided by DSM Engineering Plastics.
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 1.00 GPa
145 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort..
Tensile Modulus 1.00 GPa
145 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 NZ ESD PA12
Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of ..
Tensile Modulus 1.00 GPa
145 ksi
ASTM D 638
Cossa Polimeri ESTAPROP KUR 1520 TG05 Polypropylene, 10% Mineral Filled
PP copolymer 10% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l.
Tensile Modulus 1.00 GPa
145 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced