| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 1.03 - 2.07 GPa | 150 - 300 ksi | ASTM D790 |
|
Alcoa KAMA 2500 Prime Clear OPS, Shrink Film
(discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
|
|||
| Tensile Modulus | 1.03 - 1.38 GPa | 149 - 200 ksi | ASTM D638 |
|
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
|
|||
| Tensile Modulus | 1.03 GPa | 150 ksi | ASTM D638 |
|
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
|
|||
| Tensile Modulus | 1.03 - 1.21 GPa | 150 - 175 ksi | |
|
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works.
|
|||
| Tensile Modulus | 1.03 GPa | 149 ksi | |
|
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
|
|||
| Tensile Modulus | 1.03 - 1.21 GPa | 150 - 175 ksi | |
|
ITW Plexus Plexusâ„¢ MA330 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works..
|
|||
| Tensile Modulus | 1.03 GPa | 150 ksi | ASTM D-882 |
|
Saint-Gobain Norton® PMP Film
Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail..
|
|||
| Tensile Modulus | 1.03 GPa | 149 ksi | ASTM D638 |
|
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa..
|
|||
| Tensile Modulus | 1.03 GPa | 149 ksi | |
|
Dow Saran® 510 PVDC
SARAN® 510 resin is a copolymer of vinylidene chloride and vinyl chloride, supplied as a white free flowing powder (particle size 250 microns). It is a formulated polymer designed for extrusion int..
|
|||
| Tensile Modulus | 1.03 GPa | 149 ksi | 1 mm/min |
|
Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It ..
|
|||
| Tensile Modulus | 1.03 GPa | 150 ksi | TD; ASTM D882 |
|
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film
Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other..
|
|||