| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 10.5 GPa | 1520 ksi | |
|
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 33% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | |
|
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder
FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with ..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-2 |
|
PolyOne OnForce™ LFT LF5200-5001 EM Natural Polyolefin, Unspecified
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-1/-2 |
|
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | |
|
LATI Latilub 87/28-17ST K/15 PC, 15% Carbon Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polycarbonate (PC). Silicone / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35
Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30
Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**)
33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications su..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | 1 mm/min; ISO 527 |
|
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BG-50 PA6-GF50
Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-1 |
|
Barlog Plastics KEBATER A9030 PBT, 30% glass fiber reinforced, improved surface quality, reduced warpage
(PBT+X)-GF30Information provided by BARLOG plastics GmbH.
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-1 |
|
Barlog Plastics KEBATER BFA30 PBT, 30% glass fiber reinforced, flame retardant
PBT-GF30 FRInformation provided by BARLOG plastics GmbH.
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | 1[mm/min]; ISO 527-1/2 |
|
Akro-Plastic Akromid® T6 GF30 (3501) PPA Conditioned, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Tensile Modulus |
10.5
GPa @Temperature 23.0 °C |
1520
ksi @Temperature 73.4 °F |
DAM; ISO 527 |
|
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**)
Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | ISO 527-1/-2 |
|
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(discontinue
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Tensile Modulus | 10.5 GPa | 1520 ksi | 1mm/min; ISO 527 |
|
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
|
|||
| Tensile Modulus |
10.5
GPa @Temperature 23.0 °C |
1520
ksi @Temperature 73.4 °F |
ISO 527 |
|
DuPont Performance Polymers Rynite® FG530 NC011 PET
(Unverified Data**)
Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by..
|
|||