| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
|
Plastcom PLASTAMID® 6 GF 30 002 TS PA6 reinforced with glass fiber, heat stabilized
PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used for holders of hand tools, hobby tools, gear wheel..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 6 SGF 30 Polyamide 6, 30% Milled Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 30% of milled glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consum..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ASTM D638 |
|
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
DSM Akulon® S223-HG6U (Cond.) 33% Glass Reinforced Nylon 66 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 - 1/2 |
|
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1,-2 |
|
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® T 7323 000000 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
|
|||
| Tensile Modulus | 7.54 GPa | 1090 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS
LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability.
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East)
15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1mm/min; ISO 527 |
|
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF004AS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UF004AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
|
Polyram Metal Cap PB360B60 Nylon 6, 60% Mineral Filled, Heavy Density
60% Mineral filled, heavy density Nylon 6 for injection molding metalized part and galvanized covers.Information provided by Polyram.
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
Covestro Bayblend® T88 GF-20* Polycarbonate + SAN Glass Filled Impact Grade
Developmental productInjection molding grade20 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 7500 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
DSM Akulon® S223-HG6 (Cond.) 30% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30
Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® FE270046 BK267 Nylon 66
(Unverified Data**)
30% Glass Reinforced Polyamide 66 + Polyamide 6T/XTInformation provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 5051 (BGZ-40 FC) PA6-GF40
Product description: Grilon XE 5051 is a impact modified, heat stabilized PA 6 injection molding grade with 40% glass fiber reinforcement. Grilon XE 5051 has the following important properties: High..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
|
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Tensile Modulus | 7.51 GPa | 1090 ksi | 1 mm/min |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® LC-15H black PA12-CF15
Product description: Grilamid LC-15H black is a Polyamide 12 injection molding product reinforced with 15% carbon fibers. The product is inherently black and is only available in this color.Main Att..
|
|||
| Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
(discontinued **)
PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
|
|||
| Tensile Modulus |
7.50
GPa @Temperature 23.0 °C |
1090
ksi @Temperature 73.4 °F |
ISO 527 |
|
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
|
|||