Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 7.60 GPa
1100 ksi
STN EN ISO 527-2
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Tensile Modulus 7.60 GPa
1100 ksi
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
Tensile Modulus 7.60 - 11.7 GPa
1100 - 1700 ksi
ASTM D638
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Modulus 7.58 GPa
1100 ksi
ASTM Data
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Modulus 7.58 GPa
1100 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 7.61 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP
SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078.
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Tensile Modulus 7.57 GPa
1100 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC
LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive.
Tensile Modulus 7.58 GPa
1100 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
Tensile Modulus 7.59 GPa
1100 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC
LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant.
Tensile Modulus 7.60 GPa
1100 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..
Tensile Modulus 7.60 - 11.7 GPa
1100 - 1700 ksi
ASTM D638
3D Systems Accura® Bluestone™ Plastic for SLA® Systems
A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the ..
Tensile Modulus 7.60 GPa
1100 ksi
BASF Procom® GC40S 402 Polypropylene
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 7.60 GPa
1100 ksi
ASTM D638
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Tensile Modulus 7.58 GPa
1100 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved