| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 9.20 GPa | 1330 ksi | |
|
Plastcom SLOVAMID 6 GF 30 006/1M PA6 reinforced with 30% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 30% of milled glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and cons..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | |
|
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | |
|
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527-1/-2 |
|
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data)
This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527 |
|
Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 9.18 GPa | 1330 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527-1,-2 |
|
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modifiedInformation provided by LANXESS.
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DX07035 PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DX07035 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame retardant, Easy Molding, Internally Lubricated, Mold R..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, DRY
Description: TECHNYL® AR 130/GF is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in bla..
|
|||
| Tensile Modulus | 9.16 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
|
|||
| Tensile Modulus | 9.14 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU
LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM D638 |
|
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM D638 |
|
Plenco 6582 Phenolic, Briquette, Transfer Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM-D790 |
|
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber
30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
|
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527-1/-2 |
|
DSM Stanyl® TS250F4D Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high tempe..
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East)
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber
|
|||
| Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM D638 |
|
Plenco 7579 Phenolic, Granular, Compression Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..
|
|||