| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 9.70 GPa | 1410 ksi | |
|
Radici Radilon® A RV300R (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Tensile Modulus | 9.75 GPa | 1410 ksi | ISO 527-1/2 |
|
Radici Radilon® ARV300 (dry) Nylon 66
30% Glass-fiber reinforcedInformation provided by Radici group.
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527 |
|
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced
(discontinued **)
GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
|
|||
| Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D638 |
|
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **)
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r..
|
|||
| Tensile Modulus | 9.69 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6
LNP* KONDUIT* is a compound based on Nylon 6 resin containing thermally conductive fillers. Added feature of this material is Electrically Conductive.
|
|||
| Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D1708 |
|
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527-1,-2 |
|
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | |
|
LATI Latimass 82-06 D030 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Tensile Modulus | 9.72 GPa | 1410 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12
LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant.
|
|||
| Tensile Modulus | 9.71 GPa | 1410 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS
LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527 |
|
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0
Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:..
|
|||
| Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D638 |
|
Solvay Technyl® C216V30 30% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
|
|||
| Tensile Modulus | 9.69 GPa | 1410 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D638 |
|
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
|
|||
| Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
|
|||
| Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Tensile Modulus | 9.71 GPa | 1410 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC
LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant.
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East)
PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)...
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
|
DSM Novamid® 3021GH30 NAT PA66-GF30
30% Glass Reinforced, Heat Stabilized
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
|
|||
| Tensile Modulus | 9.74 GPa | 1410 ksi | ISO 527-1/-2 |
|
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled
Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe
|
|||