| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 10.0 GPa | 1450 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 66 GF 35 FRI 3 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
|
Premix Premi-Glas® 1205 Glass Reinforced SMC
Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
|
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus |
10.0
GPa <br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
|
1450
ksi <br>@Thickness 0.157 in,<br> Temperature 73.4 °F
|
Injection Molded; ISO 527-2/1 |
|
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Tensile Modulus |
10.0
GPa <br>@Temperature 23.0 °C
|
1450
ksi <br>@Temperature 73.4 °F
|
ISO 527 |
|
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
|
|||
| Tensile Modulus | 9.98 GPa | 1450 ksi | ASTM D638 |
|
Plenco 4759 Phenolic, Granular, Injection Molded
(discontinued **)
Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | |
|
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | |
|
LATI Latimass 82-02 D030 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | |
|
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY
Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Thermocomp PF0069 PA 6 (Europe-Africa-Middle East)
LNP* STARFLAM* PF0069 is a compound based on PA 6 resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
|
|||
| Tensile Modulus | 9.99 GPa | 1450 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 (Asia Pacific)
LNP* Thermocomp* RF006LXP is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible.
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSG-50 PA666-GF50
Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSGZ-50 PA666-GF50
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
|
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade
Information provided by Eurotec®
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
|
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR
30% Glass Reinforced, Flame Retardant (Halogen free)
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
|
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527 |
|
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
|
BLUESTAR 201-G25202 PBT, 25% Glass Filled
Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
|
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
|
Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade
(discont
Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This ..
|
|||