Polymer Property : Tensile Modulus = 17.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 17.2 GPa

@Temperature 23.9 °C
2500 ksi

@Temperature 75.0 °F
0° Direction, Dry; 8HS form; ASTM D638
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Tensile Modulus 17.2 GPa

@Temperature 23.9 °C
2500 ksi

@Temperature 75.0 °F
0° Direction, Dry; 325°F Autoclave; ASTM D638
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Tensile Modulus 17.2 GPa
2490 ksi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Tensile Modulus 17.2 GPa
2500 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PK-20CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 17.2 GPa
2490 ksi
ASTM D638
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
Tensile Modulus 17.2 GPa
2500 ksi
ASTM D638
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Modulus 17.2 GPa
2490 ksi
ASTM-D790
Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber
A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Tensile Modulus 17.2 GPa
2500 ksi
0° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Tensile Modulus 17.2 GPa
2500 ksi
Lengthwise; ASTM D638
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Tensile Modulus 17.2 GPa
2500 ksi
Lengthwise; ASTM D638
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Tensile Modulus 17.2 GPa
2500 ksi
ASTM D638
Applied Composites 8061 Polyester SMC
Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped Fibers, High Stiffness, High Fiber LoadingsInformation provided by Applied Composites Corp..
Tensile Modulus 17.2 GPa
2490 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
Tensile Modulus 17.2 GPa
2490 ksi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...
Tensile Modulus 17.2 GPa
2490 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...
Tensile Modulus 17.2 GPa
2490 ksi
ASTM-D790
Polyram Polytron A50N02 Nylon 66, Chemically Coupled 50% Long Fiber
A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Tensile Modulus 17.2 GPa
2500 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled  (discontinued **)
Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 17.2 GPa

@Temperature 100 °C
2490 ksi

@Temperature 212 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..