| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 1.03 - 1.21 GPa | 150 - 175 ksi | |
|
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works.
|
|||
| Tensile Modulus | 1.03 - 1.21 GPa | 150 - 175 ksi | |
|
ITW Plexus Plexusâ„¢ MA330 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works..
|
|||