| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 1.30 GPa | 189 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
|
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP FARADEX MS003 PP
LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | DIN 53457 |
|
Isoflon PP Polypropylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® A 30 000000 Nylon 66
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
|
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics LNP Stat-kon TE002
LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East)
LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat.
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1/-2 |
|
Styrolution Styrolux® 693 D SBC
Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
|
Borealis HB205TF Polypropylene
HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 572-2 |
|
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by ..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
Total PPC 5660 Propylene, Heterophasic Copolymer
ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
Total PPH 10099 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 1099 is a controlled-rheology homopolymer having a very narrow molecular weight distribution. PPH 10099 is characterized by high fluidity for high speed spinning on spunla..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ASTM D638 |
|
Total PPR 6523WZ Polypropylene, Nucleated Random Copolymer for Injection Molding
Impact - 6523WZ produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat - 6523WZ contains an antistat to help protect molded parts from dust acc..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1, 2 |
|
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive
Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | |
|
Covestro Baydur® GS PUR Polyurethane
Polyurethane casting system for the production of solid components. Pressureless casting into open or closed molds, fast demold times, good rot resistance. Combines easily with other materials.Infor..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® 1S XE 4224 nat PA1010
Product Description: Grilamid XE 4224 natural is a heat and UV stabilized high viscosity polyamide 1010 (PA1010), designed for extrusion. In addition the product can be used for thicker injection mo..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BS 23 PA6
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600 HWCP Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 4073 nat PA610
Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materi..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 4188 black 9992 PA612
Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | DIN 53 457 |
|
Hippe PP Polypropylene
Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min |
|
Arkema Group Orgalloy® LE 6000T Nylon Alloy, Flexible Grade (Conditioned)
LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of ..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
|
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer
This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering..
|
|||
| Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TS V0 X PA666 FR
Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr..
|
|||