| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
Polimeri Europa Edistir RK 5512G Polystyrene
UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 50 mm/min; ASTM D638 |
|
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced
Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527 |
|
Nilit FRIANYL B63 S20 Nylon 6 for injection molding
Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® 943X PC Copolymer
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL6013 PC (Europe-Africa-Middle East)
LEXAN EXL6013 is especially developed for applications requiring a high impact performance combined with an improved chemical resistance over standard polycarbonate.
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East)
LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests.
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC
LNP* Lubricomp* DL0039E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant, Easy Molding.
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | MD; ASTM D882 |
|
Eastman 9921P PET Film
(discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ASTM-D638 |
|
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527-1,-2 |
|
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend
INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527-1/-2 |
|
Mitsubishi Xantar® MX 1021 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East)
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER
PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent
|
|||
| Tensile Modulus |
2.10
GPa @Thickness 3.20 mm |
305
ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
|
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East)
Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO Data. |
|
Styron Pulse® EXT 100 ABS + Polycarbonate
PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | (1mm/min); ISO 527-2, -1A |
|
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ASTM D638 |
|
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527 |
|
Polyram RamSter PF810 PBT, Impact Modified
Impact modified PBT for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Modulus | 2.10 - 2.60 GPa | 305 - 377 ksi | |
|
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527 |
|
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527-1/-2 |
|
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | Secant; ISO 527-2 |
|
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance ..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | 1mm/min; ISO 527-1 |
|
Denka MALECCA K-600 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
|
|||
| Tensile Modulus | 2.10 GPa | 305 ksi | ASTM D638 |
|
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||