| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.30 GPa | 334 ksi | ASTM D638 |
|
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS
High flow PC+ABS material designed for local Pacific Automotive applications
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East)
High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific)
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXM101R PC (Europe-Africa-Middle East)
LEXAN FXM101R is a transparent/translucent high viscosity grade for special effects colors with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-IP ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ASTM D638 |
|
Eastman 9921P PET Injection Molded
(discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
|
|||
| Tensile Modulus |
2.30
GPa @Thickness 6.40 mm |
334
ksi @Thickness 0.252 in |
ASTM D638 |
|
SABIC Innovative Plastics Lexan® FL2000 PC
Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Apec® 1705 Polycarbonate
(discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend
(discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1/-2 |
|
Mitsubishi Xantar® 24 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Ineos ABS Lustran® Elite HH 1827
Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-2/50 |
|
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-2 |
|
Styron CALIBREâ„¢ 280-15 Polycarbonate
CALIBREâ„¢ PC Utility Grade 280-15 is a high flow opaque polycarbonate with an internal mold release system. Applications: Internal parts Electrical Electronics Lightning Information provided b..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL 731S PPE+HIPS (Europe-Africa-Middle East)
NORYL 731S is an unfilled material, with a Vicat B/120 of 135C according ISO 306. NORYL 731S cust spec 1977 has been listed for potable water applications up to 85C by the UK WFBS according BS 6920 ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527 |
|
Polyram RamShine PV101 Acrylonitrile Butadiene Styrene
General purpose ABS for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ASTM-D790 |
|
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
UV stabilized low viscosity polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® 2D 20 nat PA612
Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus |
2.30
GPa @Temperature 80.0 °C |
334
ksi @Temperature 176 °F |
ISO Data |
|
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific)
Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPS6R PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable...
|
|||