| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 124 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 124R PC
UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HF1130R PC
PC, High Flow, Mold Release, UV-Stabilized
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2R PC
Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP4R PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East)
Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS1 PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS2 PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS2R PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific)
LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 144R PC
UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer ..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HF1140 PC
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP3REU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP4EU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
|
|||