| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.40 GPa | 348 ksi | |
|
Plastcom SLOVALEN PC 71 T 20 PP, 20% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrin..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycolac® MG94 ABS (Europe-Africa-Middle East)
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
|
Nilit FRIANYL A63 S15 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPM1944 PC
Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East)
Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East)
XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited ..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
LG Chemical HI-151 ABS, Middle Impact
Information Provided by LG Chem
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP AR002XXH ABS
LNP* THERMOCOMP AR002XXH is a compound based on ABS resin containing 10% Barium Sulfate.
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
|
Styrolution Luran® S 757 G Q43 White 36609 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1mm/min; ISO 527 |
|
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1mm/min; ISO 527 |
|
Teijin Panlite® LN-1250G Flame Resistant, Translucent Polycarbonate Resin
Flame retardant and mold release grade with normal fluidity, which is suitable for injection molding applications.Applications:Electric, electronic and business machine components that need flame re..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
|
Covestro Bayblend® T65 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | |
|
Covestro Makrolon® 3108 Polycarbonate, Extrusion Grade
Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Makrolon® 6255 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6000/42 CP Nylon 6, Polymer Modified, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight ..
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 2.40 GPa | 348 ksi | ASTM D638 |
|
PolyOne Lubri-Tech™ SF-000/40T Polyphenylene Sulfide - 40% PTFE
(discontinued **)