Polymer Property : Tensile Modulus = 2.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 2.60 GPa
377 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0313 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Tensile Modulus 2.60 GPa
377 ksi
Radici Radilon® S CP400 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer
FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C.
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Tensile Modulus 2.60 GPa

@Temperature 23.0 °C
377 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® CE2055 NC010 PBT &nbsp;(Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 2.60 GPa

@Temperature 23.0 °C
377 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® S600F20 BK851 PBT &nbsp;(Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE &nbsp;(discontinued **)
Data provided by PolyOne.
Tensile Modulus 2.60 GPa
377 ksi
Ineos ABS Lustran® QE 1088 FC, Injection Grade &nbsp;(discontinued **)
Injection molding grade, high impact, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholdi..
Tensile Modulus 2.60 GPa
377 ksi
Ineos ABS LUSTROPAK® 1010 ABS, Extrusion Grade &nbsp;(discontinued **)
Extrusion grade, high stiffness.Applications: Food containers.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority..
Tensile Modulus 2.60 GPa
377 ksi
Covestro Bayblend® R-FR 390 Polycarbonate/ABS Blend &nbsp;(discontinued **)
FR-recycled grades with variable recycled content.Applications: Housings for office equipment, electrical engineering, computer sectors.Information provided by Bayer.As of 1 September 2015, Bayer Ma..
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Plaskolite Optix® PL-200 Acrylic Resin &nbsp;(discontinued **)
Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc.
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Tensile Modulus 2.60 GPa
377 ksi
LATI Latistat 87/28-06 PC
Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Tensile Modulus 2.60 GPa
377 ksi
Styrolution NOVODUR® P2H-AT ABS, Injection Grade
Standard injection molding grade, easy flow, high gloss, hard, antistatic.Applications: Telephones, household goods, video and audio industry, office equipment.
Tensile Modulus 2.60 GPa

@Thickness 4.00 mm
377 ksi

@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in..
Tensile Modulus 2.60 GPa
377 ksi
1mm/min; ISO 527-1, 2
Polyplastics TOPAS® 8007 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
Water adsorption is small and barrier properties are good, making this grade particularly suitable for package applications for products that dislike moisture. Grade 8007 has lower coefficient of el..
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)&lt
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene..
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded
AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
BLUESTAR 101G0 PBT
Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS).
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-2
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/-2
Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO..