Polymer Property : Tensile Modulus = 2.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 2.70 GPa
392 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Modulus 2.70 GPa
392 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East)
Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems.
Tensile Modulus 2.70 GPa
392 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Modulus 2.70 GPa
392 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP COLORCOMP J1000R PES (Europe-Africa-Middle East)
LNP* COLORCOMP* J1000R is a compound based on Polyethersulfone resin. Added features include : Mold Release
Tensile Modulus 2.70 GPa

@Temperature 175 °C
392 ksi

@Temperature 347 °F
ISO 527
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Tensile Modulus 2.70 GPa
392 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific)
Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives.
Tensile Modulus 2.70 GPa
392 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer
EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.70 GPa
392 ksi
cond.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced
PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1/-2
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6
PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1, -2; 1 mm/min
Lanxess Pocan® B 1701 000000 PBT
PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS.
Tensile Modulus 2.70 GPa
392 ksi
LATI Latilub 62-10T PA6
Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RX93237 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RX93237 is a compound based on Nylon 66 resin containing PTFE, Silicone, MOS2.
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1/-2
Styrolution Terluran® HH-112 Q109 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Tensile Modulus 2.70 GPa
392 ksi
ISO 527
Polyram RamLloy PBB503 PC/ABS Alloy, Flame Retardant and Heat Stabilized
Flame retardant and heat stabilized PC/ABS alloy for injection molding applications.Information provided by Polyram.
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1/-2
Covestro Bayblend® FR 3006 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradehigh heat resistanceVicat/B 120 = 110 °Ceasy flowUL-listing 94 V-1 at 1.5 mm and V-0 at 2.0 mmPreprocessingMax. Water content
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527-1,-2
Covestro Bayblend® FR3010 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527-1,-2
Covestro Bayblend® FR3100 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min
Arkema Group Lucalor® PEY 436 CPVC, Pipe Grade
LUCALOR PEY 436 is a chlorinated polyvinyl chloride compound (CPVC) developed for the extrusion of pipes for hot water supply and distribution systems.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 2.70 GPa
392 ksi
1mm/min; ISO 527
BASF Ultraform W 2320 003 BK120 Q600 POM
Ultraform W 2320 003 BK120 Q600 is a pigmented black, very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties ..
Tensile Modulus 2.70 GPa
392 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)  (Unverified Data**)
Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing ..
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1, 2
Polyplastics Duracon® M90-48 Acetal Co-polymer (POM), Antistatic, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..