| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.80 GPa | 406 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 |
|
Nilit FRIANYL B63 S Nylon 6 for injection molding
Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 5271/2 |
|
Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic
Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Appl..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min |
|
Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber
(discontinued **)
Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main applicat..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ASTM D638 |
|
Loxim 200 00V0 Polybutylene Terephthalate
Information provided by Loxim Industries
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade
PA 6, film grade, low viscosity, easy flow, additive-freeApplication Examples: flat and blown film, monofilaments, coatings
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | DIN 53457 |
|
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East)
VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East)
LNP* Thermocomp* DB0049R is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | DIN 53457 |
|
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 |
|
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and hydrolysis resistance antimony-, chlorine- and bromine-free flame retardant..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TR XE 4139 black 9231 PA*
Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | DIN 53 457 |
|
Hippe PET Polyethylene Terephthalate
Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | |
|
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe)
Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | |
|
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend
Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ASTM D638 |
|
Ashley Polymers Ashlene® 539 Nylon 66
Extrusion grade for film & monofilament.Data provided by the manufacturer
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | dry; ISO 527-1/-2 |
|
DSM Stanyl® TS271A1 PA46-RF
Aramid fiber reinforced, Wear and Friction Modified
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1, 2 |
|
Polyplastics Duracon® M270-44/M270S Acetal Co-polymer (POM), Standard, High flow, High cycle
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Tensile Modulus |
2.80
GPa <br>@Temperature 120 °C
|
406
ksi <br>@Temperature 248 °F
|
1 mm/min; ISO 527 |
|
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP
SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287.
|
|||