| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.90 GPa | 421 ksi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Rigid Extrusion 87759 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® CY5220 PC+ABS (Asia Pacific)
Non-chlorinated & non-brominated FR PC/ABS featuring good flow and impact properties. Designed for various thin wall applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East)
LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS
CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Tensile Modulus |
2.90
GPa @Temperature 23.0 °C |
421
ksi @Temperature 73.4 °F |
ISO 527 |
|
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal Homopolymer
(Unverified Data**)
Delrin® 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East)
Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM HU1004 PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 9090 PEI
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | ISO R527 |
|
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix
HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F)..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
|
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled
MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa..
|
|||
| Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
|
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding
Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi..
|
|||
| Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
|
Axiall SP-6340 Rigid PVC, Molding
Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited ..
|
|||
| Tensile Modulus | 2.90 GPa | 421 ksi | |
|
Radici Radilon® S 38F (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
|
American Polymers API 392 Polystyrene