Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2030 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 14.0 GPa
2030 ksi
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre
FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Tensile Modulus 14.0 GPa
2030 ksi
ISO.527 DIN.53455
Omnia Plastica PPS GF40 Polyphenylenesulphide
Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. ..
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Tensile Modulus 14.0 GPa
2030 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f..
Tensile Modulus 14.0 GPa
2030 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DEL34E PC (Asia Pacific)
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 14.0 GPa
<br>@Temperature 23.0 °C
2030 ksi
<br>@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement &nbsp;(discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527-1, 2
Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527
Vyncolit X613 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller..
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527-1/-2
DSM Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 14.0 GPa
2030 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40
Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Tensile Modulus 14.0 GPa
2030 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40
Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON..
Tensile Modulus 14.0 GPa
2030 ksi
1 mm/min; ISO 527
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded
BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Tensile Modulus 14.0 GPa
2030 ksi
1 mm/min; ISO 527
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded
BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
Tensile Modulus 14.0 GPa
2030 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
Tensile Modulus 14.0 GPa
2030 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527
Eurotec® Tecodur® PB70 GR40 NL100 PBT, 40% glass fiber reinforced, natural
Information provided by Eurotec®
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Tensile Modulus 14.0 GPa
2030 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 14.0 GPa
<br>@Temperature 23.0 °C
2030 ksi
<br>@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® RE5264 NC010 PET &nbsp;(Unverified Data**)
Rynite® RE5264 NC010 is a 36% glass fiber reinforced, color stabilized, modified polyethylene terephthalate.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved