Mechanical Properties Metric English Comments
Tensile Modulus 3.20 GPa
464 ksi
STN EN ISO 527-2
Plastcom PLASTAMID® 610 BT N 32 B PA610
Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o.
Tensile Modulus 3.20 GPa
464 ksi
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant
FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin..
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
Tensile Modulus 3.20 GPa
464 ksi
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling
FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packag..
Tensile Modulus 3.20 GPa
<br>@Temperature 100 °C
464 ksi
<br>@Temperature 212 °F
ISO 527
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded &nbsp;(
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Tensile Modulus 3.20 GPa
464 ksi
DIN 53457
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 1000RV PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif..
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),..
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4830 PBT+PC
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.
Tensile Modulus 3.20 GPa
464 ksi
1mm/min; ISO 527
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
Tensile Modulus 3.20 GPa
464 ksi
1mm/min; ISO 527-1, 2
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding
General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram.
Tensile Modulus 3.20 GPa
464 ksi
ISO R527
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
HexPly® M14 is a modified epoxy resin which provides good adhesion to honeycomb and foam cores. Its self-extinguishing characteristics meet the fire, smoke, and toxicity requirements of aerospace a..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 3.20 GPa
464 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437G25M5CL Glass/Mineral Reinforced Coupled
Tensile Modulus 3.20 GPa
464 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-2
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable
During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit..
Tensile Modulus 3.20 GPa
464 ksi
Parylene Coating Services C Poly (P-Xylylene)
Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-..
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-2
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled
Heat stabilizedInformation provided by PolyPlastic Group.
Tensile Modulus 3.20 GPa
464 ksi
ISO 527 - 1 &amp; - 2
Asahi Kasei Tenac® SH410 Homopolymer Acetal Resin
General purpose grade, high impact, high elongation, medium viscosityInformation provided by Asahi Kasei Corporation.
Tensile Modulus 3.20 GPa
464 ksi
1mm/min; ISO 527-2/1A/1
SYNTHOS Krasten® 172 General Purpose Polystyrene