| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Tensile Modulus | 3.45 GPa | 501 ksi | chs 2 in/min; ASTM D638 |
|
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
|
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS
LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers.
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | Dried; ISO 527 |
|
Manifattura Cattaneo PA 6.6 Nylon
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | |
|
Ineos ABS Lustran® SAN 31 51
Key Features:UnfilledSuitable processing methods:Injection molding
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DD0001 PC
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66
LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus |
>=
3.45
GPa <br>@Temperature 23.9 °C
|
>=
500
ksi <br>@Temperature 75.0 °F
|
|
|
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation ..
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | |
|
Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
|
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
|
|||
| Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
|
Quantum PEEK
Information provided by Quantum Advanced Engineering Plastics
|
|||