| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.20 GPa | 319 ksi | |
|
Plastcom SLOVALEN PC 51 T 25 PP, 25% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527 |
|
Polycasa PC
QUINN PC sheets have excellent optical properties and a brilliant surface. The QUINN PC range contains sheets that are easy to fabricate and show exceptional performance at both low and high tempera..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycolac® FR30U ABS
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS
High impact and ductility at 73F and -20F. For thin-wall applications.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min |
|
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light ..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
|
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
|
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall
Information Provided by LG Chem
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral
PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific)
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer
LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527 |
|
Styrolution Novodur® E309 ABS
Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ISO Data. |
|
Styron CALIBREâ„¢ IM 401 11 Polycarbonate, Impact Modified
CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East)
NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | DIN 53457 |
|
Zell-Metall Engineering Plastics Zellamid 1200 G
Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM-D790 |
|
Polyram RamTal PM1409 Acetal, PTFE Filled
Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind.
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Bayblend® T65 AT PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 3959 nat PA610
Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
|
Aclo Accutech Polypropylene Homopolymer HP0339C40L Calcium Reinforced |
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
|
Aclo Accutech Polypropylene Homopolymer HP0339C40L1 Calcium Reinforced |
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
|
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant
Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
|
|||
| Tensile Modulus | 2.20 GPa | 319 ksi | TD; ASTM D882 |
|
Eastman 9921W PET Film
(discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
|
|||