| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.30 GPa | 334 ksi | ASTM D638 |
|
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Lexan® AD4820 PC
LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Plastcom SLOVAMID 6 MI PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1/-2 |
|
Mitsubishi Xantar® MX 1071 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1/-2 |
|
Mitsubishi Xantar® MX 2021 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | DIN 53457 |
|
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1mm/min; ISO 527 |
|
Styrolution Terluran® GP-22 ABS
Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-2/50 |
|
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-2/50 |
|
Styron CALIBREâ„¢ 703-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
|
Styron EMERGEâ„¢ 4510-15 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific)
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ 1080 DVD Polycarbonate
CALIBREâ„¢ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | |
|
Covestro Makrolon® 6385 Polycarbonate, Injection Grade
Low viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1 |
|
Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact
PBT+PCInformation provided by BARLOG plastics GmbH.
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-2 |
|
CENTROPLAST CENTROPHEN Polyphenylene ether modified
This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include fittings, drive components for domestic appliances, and compon..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min |
|
Arkema Group Kynar® 6000 HDC N 119 PVDF
(discontinued **)
Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m..
|
|||
| Tensile Modulus | 2.30 GPa | 334 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East)