Polymer Property : Tensile Modulus = 340 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Quantum PPSU
Information provided by Quantum Advanced Engineering Plastics
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1300-22 Polycarbonate Resin
Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1201-22 Polycarbonate Resin
Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin
Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Tensile Modulus 2.34 GPa
340 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 2061-22 Polycarbonate
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Tensile Modulus 2.34 GPa
340 ksi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4310-22 Polycarbonate
EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn..
Tensile Modulus 2.34 GPa
340 ksi
2 in/min; ASTM D638
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Modulus 2.34 GPa
340 ksi
2 in/min; ASTM D638
Styron CALIBREâ„¢ 303 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Westlake Plastics Radel® R Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU)
TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Ensinger TECASON™ P Polyphenylsulfone (PPSU)
TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties.
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Asahi Kasei Thermylene® P-10FG-2100 10% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the..