| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.35 GPa | 341 ksi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East)
LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® 9945A PC (Asia Pacific)
Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EX7681T_ PC (Europe-Africa-Middle East)
LEXAN EX7681T is a coextrusion product which is highly UV stabilised exhibiting low plate out and improved outdoor weathering of LEXAN sheet.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD141 PC (Europe-Africa-Middle East)
LEXAN FXD141 is a transparent/translucent medium viscosity grade for light diffusion effects. The color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD143R PC (Europe-Africa-Middle East)
LEXAN FXD143R is a transparent/translucent medium viscosity grade for light diffusion effects. UV-stabilized. The color package may affect performance.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD921A PC (Europe-Africa-Middle East)
LEXAN FXD921A is a transparent/translucent, medium viscosity, flame retardent grade for light diffusion special effects. Color package may affect performance.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXE164R PC (Europe-Africa-Middle East)
LEXAN FXE164R is a transparent/translucent medium viscosity grade for special effects with fluorescent appearance. FDA compliant. Color package may affect performance. LEXAN FXE164R contains a rel..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific)
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific)
Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East)
Low-viscosity multi-purpose grade having low levels of ionics species.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific)
Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® SLX2571T PC Copolymer (Europe-Africa-Middle East)
Transparent weatherable PC copolymer for blowmolding/extrusion.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East)
PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics PC0800 PC (Europe-Africa-Middle East)
PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics PC1803R PC (Asia Pacific)
PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
|
|||
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||