| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 124R PC
UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HF1130R PC
PC, High Flow, Mold Release, UV-Stabilized
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HF1140R PC
High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East)
Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS1S PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS2 PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HPS2R PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East)
XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 144R PC
UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer ..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HF1140 PC
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2NR PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® ML4248 PC
Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Extrusion grade. Transparent, transluscent and opaque colors.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | ISO 527-2/1A/1 |
|
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
|
|||
| Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||