| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.45 GPa | 355 ksi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | STN EN ISO 527-2 |
|
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | Type I; ASTM D638 |
|
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EX2079X PC (Europe-Africa-Middle East)
Lexan* EX2079X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPS7R PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific)
LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | |
|
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant
FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min |
|
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | |
|
Radici Radiflam® S FR (cond.) Nylon 6
PA6 flame retardant injection molding grade. Halogen and phosphorus free. Natural color. Suitable for monofilament extrusion.Information provided by Radici group.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | ASTM D638 |
|
Global ABS-1805 General Purpose ABS
(discontinued **)
Information provided by Global Polymers Corporation.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | |
|
Ineos Styrenics Polystyrene 147F (NAFTA)
An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific)
LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East)
NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527 |
|
Wico Plast Wicolon 805 Polycarbonate
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Apec® FR1892 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | |
|
Dow SiLK™ I 130 Semiconductor Dielectric Resin
SiLK™ I 130 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 130 is compatible with..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | |
|
Dow SiLK™ I300 140 Semiconductor Dielectric Resin
SiLK™ I300 140 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 140 is compatibl..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min |
|
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned)
Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema.
|
|||
| Tensile Modulus |
2.45
GPa @Temperature 80.0 °C |
355
ksi @Temperature 176 °F |
ISO Data |
|
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..
|
|||
| Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/2 |
|
BLUESTAR BS090 Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||