| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
|
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
|
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
|
Nilit FRIANYL B63 KV40 Nylon 6 for injection molding, 40% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC
LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by ..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ASTM D638 |
|
PolyOne Edgetek® ES-15GF/000 RED Polyethersulfone - 15% Glass Fiber Reinforced
(discontinued **)
Data provided by PolyOne.
|
|||
| Tensile Modulus |
4.50
GPa <br>@Thickness 0.100 mm
|
653
ksi <br>@Thickness 0.00394 in
|
TD; ISO 527 |
|
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
|
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
|
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance, good surface, good flowability (Easy Flow), low warpage
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow)
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, Conditioned
Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM HU2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East)
GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
|
Polyram PlusTek PB300G2 Nylon 6 for Injection Molding, 10% Glass-Fiber Reinforced
10% Glass-fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR
Information provided by EMS Grivory
|
|||
| Tensile Modulus |
4.50
GPa <br>@Temperature 200 °C
|
653
ksi <br>@Temperature 392 °F
|
ISO 527-1/-2 |
|
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | Secant; ISO 527-2 |
|
ExxonMobil Exxtral™ HMU 405 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSG-15/4 PA666-GF15
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
|
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva..
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1 |
|
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
PBT-GF10Information provided by BARLOG plastics GmbH.
|
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
|
DSM Arnite® TB6 260 PBT-GB30 |
|||
| Tensile Modulus | 4.50 GPa | 653 ksi | |
|
LATI Latimass 82-05 D040 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||