| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 4.60 GPa | 667 ksi | ISO 527 |
|
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Asia Pacific)
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus |
4.60
GPa <br>@Temperature 80.0 °C
|
667
ksi <br>@Temperature 176 °F
|
1 mm/min; ISO 527 |
|
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP
SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DDF029 PC (Asia Pacific)
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant, Glass Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer
LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10
LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DDF029 PC
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East)
10% GF FR PBT/PC Blend
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific)
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | ASTM D 638 |
|
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled
PP homopolymer 20% chemically coupled glass fiber reinforcedInformation provided by Cossa Polimeri S.r.l.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | ISO 527-1/-2 |
|
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable ..
|
|||
| Tensile Modulus |
4.60
GPa <br>@Temperature 160 °C
|
667
ksi <br>@Temperature 320 °F
|
ISO 527-1/-2 |
|
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 50%RH; ISO 527-1/-2 |
|
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | ASTM D638 |
|
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||
| Tensile Modulus |
4.60
GPa <br>@Temperature 80.0 °C
|
667
ksi <br>@Temperature 176 °F
|
ISO Data |
|
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and ..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | ISO 527-1/-2 |
|
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | cond.; ISO 527 |
|
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced
20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following ..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 1mm/min; ISO 527 |
|
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry)
Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability.
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVALEN PH 79 GF 20 Polypropylene Homopolymer, 20% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
|
|||
| Tensile Modulus | 4.60 GPa | 667 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East)
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
|
|||