| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.80 GPa | 406 ksi | ASTM D638 |
|
Nilit Polynil® P100 Medium Viscosity Nylon 66
Description: Polynil P100 is a grade has a viscosity that has been optimized for monofilament extrusion for high strength monofilaments.Key characteristics: Viscosity number 200 gr/cm3Excellent melt..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific)
CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 |
|
Nilit FRIANYL B63 S Nylon 6 for injection molding
Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 |
|
Grupo Repol Dinalon® B1S25 H PA6 Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | |
|
LATI Latilub 66-20T PA66, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 |
|
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP RP002 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RP002 is a compound based on PA 66 resin containing PTFE, Silicone: Added features include; Internallly Lubricated.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized.
|
|||
| Tensile Modulus |
2.80
GPa <br>@Temperature 23.0 °C
|
406
ksi <br>@Temperature 73.4 °F
|
|
|
Hexcel® HexPly® 954-3 Curing Cyanate Resin
HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | |
|
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend
Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | cond; ISO 527-1/-2 |
|
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR
Information provided by EMS Grivory
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TR 30 nat PA*
Product description: Grilamid TR 30 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 natural offers outstanding properties..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TR XE 4139 black 9231 PA*
Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**)
Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527 - 1 & - 2 |
|
Asahi Kasei Tenac® LA543 Homopolymer Acetal Resin
Excellent friction and wear on metals and plastics, except POM.Information provided by Asahi Kasei Corporation.
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | |
|
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend
Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | dry; ISO 527-1/-2 |
|
DSM Stanyl® TS271A1 PA46-RF
Aramid fiber reinforced, Wear and Friction Modified
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
|
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | 1 mm/min |
|
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface..
|
|||
| Tensile Modulus | 2.80 GPa | 406 ksi | ASTM D638 |
|
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||