| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 3.00 GPa | 435 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific)
CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
|
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding
Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Tensile Modulus |
3.00
GPa <br>@Temperature 23.0 °C
|
435
ksi <br>@Temperature 73.4 °F
|
ISO 527 |
|
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min |
|
Arkema Group Oroglas® MI-2T Acrylic
(discontinued **)
OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP JZL012 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JZL012 is a compound based on Polyethersulfone resin containing Proprietary Filler, PTFE. Added features include: Internally Lubricated.
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE
High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method).
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 7
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15
Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
|
DSM Stanyl® TE351 PA46 FR(17)
Flame Retardant, Heat Stabilized
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6000 S Nylon 6, Finely Crystalline, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6
Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® XE 4185 black 9453 PA*
Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
|
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 - 1 & - 2 |
|
Asahi Kasei Tenac® 3013A Homopolymer Acetal Resin
Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation.
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527 |
|
BASF Ultramid® 1000-2 NF2001 PA66 (Dry)
Ultramid 1000-2 NF2001 is a general purpose PA6/6.
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
|
DSM Akulon® S240-C Nylon 66 (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 303 Natural FA PA66, DRY
Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe Product Applications: TECHNYL® A 303 Natural FA offers three main advantages: high impact resistanc..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 50 mm/min; ASTM D638 |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527-1 |
|
Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled
SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.Information ..
|
|||
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY
Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit..
|
|||