| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO.527 DIN.53455 |
|
Omnia Plastica Akulon® PA 66 - Akulon 66 - Dry
Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
|
|||
| Tensile Modulus | 3.20 - 3.38 GPa | 464 - 490 ksi | ASTM D638 |
|
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer
Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific)
LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ASTM Data |
|
Americas Styrenics Styron® 685 Polystyrene
(discontinued **)
STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1,-2 |
|
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | |
|
LATI Latigray 75/4-01 CX/45 PBT
Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 1000V PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in ..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM HU1100 PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
|
Styrolution PS 124 N/L GPPS
Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2/50 |
|
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
|
Polyram RamTough PZ333G2 Polycarbonate, 10% Glass Fiber, Flame Retardant
10% glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527; DIN 53452 |
|
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH
Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1/-2 |
|
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1/-2 |
|
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Tensile Modulus |
3.20
GPa <br>@Temperature 23.0 °C
|
464
ksi <br>@Temperature 73.4 °F
|
EN ISO 527 |
|
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
|
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 - 1 & - 2 |
|
Asahi Kasei Tenac® 4010 Homopolymer Acetal Resin
General purpose grade, high impact, high elongation, medium viscosityInformation provided by Asahi Kasei Corporation.
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2 |
|
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable
During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit..
|
|||
| Tensile Modulus |
3.20
GPa <br>@Temperature 23.0 °C
|
464
ksi <br>@Temperature 73.4 °F
|
ISO 527 |
|
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527-2/1A/1 |
|
SYNTHOS Krasten® 171 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high ..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527-2/1A/1 |
|
SYNTHOS Krasten® 172 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1/-2 |
|
DSM Arnite® T06 204 SN PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2/1A/1 |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..
|
|||