| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 3.40 GPa | 493 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID 6 GB 30 HI PA6 reinforced with glass beads, improved impact strength
PA 6 for injection molding, reinforced with 30% glass beads, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
|
Polycasa PS
QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
|
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..
|
|||
| Tensile Modulus |
3.40
GPa <br>@Temperature 23.0 °C
|
493
ksi <br>@Temperature 73.4 °F
|
ISO 527 |
|
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ASTM D638 |
|
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **)
Data provided by PolyOne.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
|
Lanxess Durethan® B 30 S FN40 000000 Nylon 6
PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | cond.; ISO 527-1, -2; 1 mm/min |
|
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | |
|
LATI Latimass 75/4-04 D009 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min, Type 1A; ISO 527-2 |
|
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
|
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS)
Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific)
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
|
Polyram RamTal PMH2022 Polyacetal Homopolymer for Injection Molding
General purpose polyacetal homopolymer for injection molding applications, MFI 22.Information provided by Polyram.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ASTM-D790 |
|
Polyram RamTough PZ322G2 Polycarbonate, 10% Glass Fiber
10% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | dry; ISO 527-1/-2 |
|
DSM Novamid® 1010C2 PA6
Easy Molding Grade
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BG-15 PA6-GF15
Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | dry; ISO 527-1/-2 |
|
DSM Stanyl® TS350 PA46 FR(17)
Unreinforced, Flame Retardant
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**)
Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
|
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion
Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar.
|
|||
| Tensile Modulus |
3.40
GPa <br>@Temperature 23.0 °C
|
493
ksi <br>@Temperature 73.4 °F
|
ISO 527 |
|
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
|
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded
Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ASTM D638 |
|
Aclo Accutech Polypropylene Copolymer CP0437G30CL Glass Reinforced Coupled |
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 - 1 & - 2 |
|
Asahi Kasei Tenac® 7054 Homopolymer Acetal Resin
High-flow grade with high crystallization rate for higher productivity.Information provided by Asahi Kasei Corporation.
|
|||
| Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 - 1 & - 2 |
|
Asahi Kasei Tenac® SH510 Homopolymer Acetal Resin