Polymer Property : Tensile Modulus = 5.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 5.10 GPa
740 ksi
Plastcom SLOVALEN PH 69 GF 20 T 10 PP, 20% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre and 10 % Talc, contains themodifier of mechanical properties.Increased strength in comparison with ..
Tensile Modulus 5.10 GPa
740 ksi
STN EN ISO 527-2
Plastcom SLOVALEN PH 69 GF 25 Polypropylene Homopolymer, 25% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Tensile Modulus 5.10 GPa
740 ksi
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Tensile Modulus 5.10 GPa
740 ksi
ASTM D638
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
Conditioned; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Tensile Modulus 5.10 GPa
740 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber
PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable
Tensile Modulus 5.10 GPa
740 ksi
ISO 527-1/-2
Lanxess Pocan® KU 1-7625 901510 PBT + PC, 20% Glass Fiber
PBT+PC, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
Tensile Modulus 5.10 GPa
740 ksi
LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced
EMI shielding product based on Polycarbonate (PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Tensile Modulus 5.10 GPa
740 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Tensile Modulus 5.10 GPa
740 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL IGN5531 PPE+PS
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
Tensile Modulus 5.10 GPa
740 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific)
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
Tensile Modulus 5.10 GPa
740 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East)
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
Tensile Modulus 5.10 GPa
740 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP
LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app..
Tensile Modulus 5.10 GPa
740 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.
Tensile Modulus 5.10 GPa
740 ksi
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix
HexPly® M12 is a good performance, self extinguishing, tough epoxy matrix for use in helicopter blades. It exhibits good fatigue life and hot/wet performances up to 100ºC. HexPly® M12 is supplied..
Tensile Modulus 5.10 GPa
740 ksi
ISO 527-1/-2
Covestro Bayblend® T88 GF-10* Polycarbonate + SAN Glass Filled Impact Grade
Developmental productInjection molding grade10 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 5100 MPaVicat/B 120 = 134 °CPreprocessingMax. Water content
Tensile Modulus 5.10 GPa
740 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.10 GPa
740 ksi
ISO 527
Azoty Tarnow™ TARNOFORM 300 GF2 POM
10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Tensile Modulus 5.10 GPa
740 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Conditioned, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Tensile Modulus 5.10 GPa
740 ksi
1mm/min; ISO 527
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
Tensile Modulus 5.10 GPa
740 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper
Information provided by Asahi Thermofil
Tensile Modulus 5.10 GPa
740 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0860 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Tensile Modulus 5.10 GPa

@Temperature 175 °C
740 ksi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Tensile Modulus 5.10 GPa
740 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha..