| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
|
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data)
Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
|
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data)
Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific)
Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available ..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | MD; ISO 527 |
|
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
|
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY
Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
|
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber
A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris..
|
|||
| Tensile Modulus | 5.50 GPa | 797 ksi | ASTM D638 |
|
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
|
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**)
13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min |
|
Arkema Group Orgalloy® RS 6620 Nylon 66 Alloy, 20% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527/4 |
|
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | cond.; ISO 527 |
|
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced
25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1mm/min; ISO 527 |
|
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade.
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
|
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ASTM D638 |
|
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
|
|||