Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 5.58 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 5.58 GPa
809 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
Tensile Modulus 5.58 GPa
809 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
Tensile Modulus 5.58 GPa
809 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP
LNP* THERMOCOMP* MFB429 is a compound based on Polypropylene resin containing 10% Glass Fiber, 20% Glass Bead. Added features of this material include: Chemically Coupled, Flame Retardant.
Tensile Modulus 5.58 GPa
809 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP (Asia Pacific)
LNP* Thermocomp* MFB429 is a compound based on Polypropylene resin containing Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant.
Tensile Modulus 5.58 GPa

@Temperature 100 °C
809 ksi

@Temperature 212 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..