| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 3.79 GPa | 550 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
|
PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D822 |
|
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® LBTW Polyester Film, 92 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge
Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® OL2 Polyester Film, 100 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
|
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML..
|
|||
| Tensile Modulus | 3.79 - 5.17 GPa | 550 - 750 ksi | ASTM D638 |
|
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice..
|
|||
| Tensile Modulus | 3.79 GPa | 550 ksi | TM R050-36 |
|
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
|
|||