Mechanical Properties Metric English Comments
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 7.50 GPa
1090 ksi
Plastcom SLOVASTER® B1 GF 20 000/1 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticit..
Tensile Modulus 7.50 GPa

@Temperature 23.0 °C
1090 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527-1/-2
Lanxess Pocan® KU 1-7635 901510 PBT + PC, 30% Glass Fiber
PBT+PC, 30% glass fibers, injection molding, low tendency to warp, improved surface finish
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This ..
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66
LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding.
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is ..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3..
Tensile Modulus 7.50 GPa
1090 ksi
1mm/min; ISO 527-2
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced
Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527-1/-2
DSM Akulon® M-1016 (Cond.) 33% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527-1/-2
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Modulus 7.50 GPa
1090 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35
Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Tensile Modulus 7.50 GPa
1090 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Tensile Modulus 7.50 GPa
1090 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Tensile Modulus 7.50 GPa
1090 ksi
cond.; DIN 53 457
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
Tensile Modulus 7.50 GPa
1090 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded
Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded
Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527-2/1
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Conditioned, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Tensile Modulus 7.50 GPa
1090 ksi
STN EN ISO 527-2
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl..
Tensile Modulus 7.50 GPa
1090 ksi
1mm/min; ISO 527
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527-1/-2
DSM Arnite® TV4 440 KL PBT/PET Blend-20% Glass Reinforced (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b..
Tensile Modulus 7.50 GPa
1090 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..
Tensile Modulus 7.50 GPa

@Temperature 23.0 °C
1090 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
Copyright © lookpolymers.com All Rights Reserved