Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 7.58 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
PolyOne Nymax™ GMF 600 A 40 Storm Grey Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Modulus 7.58 GPa
1100 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU)
Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 7.58 GPa
1100 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 7.58 GPa
1100 ksi
ASTM Data
Dow Questra® QA804 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM Data
Dow Questra® WA207 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM Data
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific)
LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced
Tensile Modulus 7.58 GPa
1100 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific)
LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System.
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Tensile Modulus 7.58 GPa
1100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific)
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
Tensile Modulus 7.58 GPa
1100 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications &am
Data provided by PolyOne.
Copyright © lookpolymers.com All Rights Reserved