Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 725 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 5.00 GPa
725 ksi
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads
FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
Tensile Modulus 5.00 GPa
725 ksi
STN EN ISO 527-2
Plastcom SLOVAMID 66 W 40 Polyamide 66, 40% Mineral Filled
FeaturesPA 66 with the content of 40% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel ..
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Nilit FRIANYL A63 GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 5.00 GPa
725 ksi
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 5.00 GPa

@Thickness 0.100 mm
725 ksi

@Thickness 0.00394 in
MD; ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-1/-2
DSM Akulon® S223-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 66 (North America)  (discontinued **)&
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 5.00 GPa
725 ksi
cond.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
Tensile Modulus 5.00 GPa
725 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY
Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind..
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V03505 PPE+HIPS
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V03550 PPE+HIPS
Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 5.00 GPa
725 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 815F PBT+PET
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, ..
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Polyram RamLloy PN300G4 PPE/PS Alloy, 20% Glass Fiber
PPE/PS alloy, 20% glass fiber reinforced for injection molding applications.Information provided by Polyram.
Tensile Modulus 5.00 GPa

@Temperature 120 °C
725 ksi

@Temperature 248 °F
ISO 527-1/-2
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.00 GPa
725 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Tensile Modulus 5.00 GPa
725 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Tensile Modulus 5.00 GPa
725 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Conditioned, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Tensile Modulus 5.00 GPa
725 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform..
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66
Information provided by A. Schulman.
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-2
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber
CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element..
Tensile Modulus 5.00 GPa
725 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p..
Tensile Modulus 5.00 GPa
725 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East)
15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Copyright © lookpolymers.com All Rights Reserved