| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
| Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® LR900G2 PC (Europe-Africa-Middle East) PC 20% GF Recycle Grade, Preliminary properties |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527, ASTM D638 |
| Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® HFD4472 PC (Asia Pacific) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
| DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 527-1,-2 |
| Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 527-1,-2 |
| Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | Conditioned; ISO 527-1/-2 |
| Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 Type 1A |
| Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66 LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
| Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
| CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | dry; ISO 527-1/-2 |
| EMS-Grivory Grivory® LV-2H PA12-GF20 Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | DAM; ISO 527-1/-2 |
| DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 50%RH; ISO 527-1/-2 |
| DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
| Eurotec® Tecodur® PB70 GR15 BK EF PBT, 15% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
| CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min |
| Arkema Group Orgalloy® RS 6620 Nylon 66 Alloy, 20% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
| Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ASTM D638 |
| Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | cond.; ISO 527 |
| Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced 25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
| Eurotec® Tecomid® NB40 KG30 NL 0G PA6, 30% glass fiber/glass bead reinforced, natural Information provided by Eurotec® |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® 3412ECR PC Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||