| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 8.50 GPa | 1230 ksi | |
|
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength
FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength ..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | STN EN ISO 527-2 |
|
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized
PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 50 mm/min; ASTM D638 |
|
Ovation Polymers Opnyl OP66GF50 Nylon 66
Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
|
|||
| Tensile Modulus |
8.50
GPa @Temperature 23.0 °C |
1230
ksi @Temperature 73.4 °F |
ISO 527-2/1 |
|
PolyOne Bergamid™ A70 G25 H natur TM-X Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527-1,-2 |
|
Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fiber, injection molding, improved flowability, hydrolysis stabilized, improved surface finish, GIT/WITInformation provided by LANXESS.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527-1,-2 |
|
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | |
|
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East)
XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP PFW53U PA 6
LNP THERMOCOMP* PFW53U is a compound based on Nylon 6 resin containing 15% Glass Fiber, 15% Wollastinite. Added features of this material include: UV Stabilized.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP PFW53U PA 6 (Asia Pacific)
LNP* THERMOCOMP* PFW53U is a compound based on Nylon 6 resin containing Glass Fiber, Mineral. Added features of this material include: UV Stabilized.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East)
LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Thermocomp PF006ES PA 6 (Europe-Africa-Middle East)
Hydrolysis Resistant Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
|
Plenco 3509 Phenolic, Granular, Injection Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
|
Plenco 7591 Phenolic, Briquette, Injection Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
|
|||
| Tensile Modulus | 8.50 - 10.0 GPa | 1230 - 1450 ksi | ISO 527 |
|
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
DSM Arnite® TV4 241 SN PBT-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
DSM Arnite® TV4 244 S PBT-GF20 FR
20% Glass Reinforced, Flame Retardant
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BG-40 FC PA6-GF40
Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
|
Eurotec® Tecomid® NA40 GR25 NL XA 42 PA 6.6 25% glass fiber reinforced, UL94 V0, red phosphorus
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
|
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
|
Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1, 2 |
|
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||