Mechanical Properties Metric English Comments
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-2
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Modulus 9.00 GPa
1310 ksi
50 mm/min; ASTM D638
Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned
Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Tensile Modulus 9.00 GPa
1310 ksi
50 mm/min; ASTM D638
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Dry
Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m..
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527, ASTM D638
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-2/1A
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber
Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr..
Tensile Modulus 9.00 GPa
1310 ksi
Type I, 5.0 mm/min; ISO 527
PolyOne Edgetek® QT020GFS/000 FR NATURAL - OBSOLETE Syndiotactic Polystyrene (SPS)
Information provided by PolyOne
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled  (discontinued **)
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527
Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-2
Pasargad Polymer Peyvand Pasamid 3P-H1145B Nylon 6, 45% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-1/-2
DSM Akulon® K-FHGM35 (Dry) 40% Glass/Mineral Reinforced, Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527
Grupo Repol Dinalon® B1S25 G30 PA6 30% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Tensile Modulus 9.00 GPa
1310 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
Tensile Modulus 9.00 GPa
1310 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Tensile Modulus 9.00 GPa
1310 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
Tensile Modulus 9.00 GPa
1310 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF006ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Tensile Modulus 9.00 GPa
1310 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release...
Tensile Modulus 9.00 GPa
1310 ksi
1mm/min; ISO 527
Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 30 % filler. Improved stiffness and high fluidity realizes a thin wall..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Plenco 2300 Phenolic, Granular, Compression Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-1/-2
DSM Akulon® S223-HM8 (Dry) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 9.00 GPa
1310 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66  (Unverified Data**)
30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers
Tensile Modulus 9.00 GPa
1310 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-1/-2
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..