Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 9.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527
Radici Radilon® A GV H0 30P Nylon 66-GF30
Automotive cooling liquid resistant PA66-GF30 grade designed to resist even in more severe operating condition. Indicated as "top of the class" material.Information provided by Radici group.
Tensile Modulus 9.70 GPa
1410 ksi
Radici Radilon® A RV300R (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/2
Radici Radilon® SRV300 (dry) Nylon 6
Glass-fiber reinforcedInformation provided by Radici group.
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced  (discontinued **)
GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/-2
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/-2
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
Tensile Modulus 9.70 GPa
1410 ksi
LATI Latigray 82-04 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Tensile Modulus 9.70 GPa
1410 ksi
LATI Latimass 82-06 D030 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0
Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:..
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXC PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL36SXC is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East)
LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO
LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East)
LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled.
Tensile Modulus 9.70 GPa
1410 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East)
PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)...
Tensile Modulus 9.70 GPa
1410 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSG-30 PA666-GF30
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl..
Tensile Modulus 9.70 GPa
1410 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/-2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Tensile Modulus 9.70 GPa
1410 ksi
dry; DIN 53 457
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
Tensile Modulus 9.70 GPa
1410 ksi
dry; ISO 527-1/-2
DSM Novamid® 3021GH30 BK629 PA66-GF30
30% Glass Reinforced, Heat Stabilized
Tensile Modulus 9.70 GPa
1410 ksi
LATI Latigray 82-05 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Tensile Modulus 9.70 GPa
1410 ksi
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri..
Tensile Modulus 9.70 GPa
1410 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved